CPC C01B 32/21 (2017.08) [H01M 4/366 (2013.01); H01M 4/583 (2013.01); H01M 10/0525 (2013.01); C01P 2004/32 (2013.01); C01P 2004/51 (2013.01); C01P 2004/61 (2013.01); C01P 2006/12 (2013.01); C01P 2006/14 (2013.01); H01M 2004/021 (2013.01); H01M 2004/027 (2013.01)] | 17 Claims |
1. Spherically-shaped coated graphite comprising:
spherically-shaped graphite in which primary particles with an equivalent spherical diameter of not more than 0.8 μm have a volume ratio of more than 40.0% and not more than 70.0%, and primary particles with an equivalent spherical diameter of not less than 1.5 μm and not more than 3.0 μm have a volume ratio of not less than 3.0% and not more than 17.0%, in a particle size distribution of primary particles that is obtained using X-ray computed tomography; and
a carbonaceous substance covering the spherically-shaped graphite,
wherein a pore volume of pores with a pore size of not less than 7.8 nm and not more than 36.0 nm is not more than 0.017 cm3/g, and
a mass of infiltrated dibutyl phthalate in the spherically-shaped coated graphite is less than 0.70 g/cm3.
|