CPC H01L 33/502 (2013.01) [C09K 11/06 (2013.01); H01L 31/02168 (2013.01); H01L 31/0481 (2013.01); B82Y 20/00 (2013.01); B82Y 40/00 (2013.01); C09K 2211/14 (2013.01); H01L 33/56 (2013.01); H01L 2933/0041 (2013.01)] | 12 Claims |
1. A solar spectral wavelength converting material comprising an aluminum hydroxide to which 1-pyrenecarboxylic acid is anchored by a process comprising combining an aluminum hydroxide precursor and 1-pyrenecarboxylic acid in a solvent having a boiling point of at least 200° C. and heating the mixture, followed by removing air and moisture and purging with inert gas, then heating the resulting mixture at a temperature and for a time sufficient to perform thermal decomposition.
|