CPC C07C 209/18 (2013.01) [B01J 23/72 (2013.01); B01J 35/023 (2013.01); B01J 37/0236 (2013.01); B01J 37/031 (2013.01); B01J 37/04 (2013.01); B01J 37/06 (2013.01); C07C 211/48 (2013.01); C07C 2523/72 (2013.01)] | 2 Claims |
1. A method for producing a catalyst containing Cu, Zn and Al, comprising: adding an aqueous sodium carbonate solution and a mixture of aqueous copper nitrate and zinc nitrate solution to an aqueous suspension of aluminum oxide, while maintaining a pH of 7.5-8.5, at a temperature of 60-80° C., wherein the mixture of aqueous copper nitrate and zinc nitrate solution is adjusted before the addition to a pH of <1, the resulting suspension containing Cu, Zn and Al is subsequently washed, then dried, the solid obtained therefrom is calcined.
|