| CPC C09J 7/35 (2018.01) [C08K 5/01 (2013.01); C08L 23/0815 (2013.01); C08L 23/0853 (2013.01); C08L 23/16 (2013.01); C08L 91/06 (2013.01); C08L 2201/08 (2013.01); C08L 2205/025 (2013.01); C08L 2205/035 (2013.01); C08L 2314/06 (2013.01); C09J 2301/304 (2020.08); C09J 2301/414 (2020.08); C09J 2423/04 (2013.01); C09J 2423/10 (2013.01); C09J 2423/16 (2013.01); C09J 2491/00 (2013.01)] | 14 Claims |
|
1. A hot-melt adhesive comprising:
a copolymer (A) comprising a mixture of a propylene/ethylene copolymer that is prepared with a metallocene catalyst (A1), an ethylene/octene copolymer that is prepared with a metallocene catalyst (A2), and a metallocene-type ethylene/hexene copolymer (A3);
a copolymer of ethylene and carboxylate esters having ethylenically unsaturated double bonds (B) comprising an ethylene/vinyl acetate copolymer (B1);
a tackifying resin (C); and
a wax (D), wherein:
the propylene/ethylene copolymer (A1) is present in an amount of from 5 to 40 parts by weight, based on 100 parts by total weight of the hot-melt adhesive,
the ethylene/octene copolymer (A2) is present in an amount of from 10 to 40 parts by weight, based on 100 parts by total weight of the hot-melt adhesive, and
the hot-melt adhesive has a viscosity of from 500-3000 mPas at 150° C., measured with Brookfield Viscometer, spindle 27.
|