| CPC B32B 37/12 (2013.01) [B30B 9/28 (2013.01); B32B 7/12 (2013.01); B32B 15/043 (2013.01); B32B 15/18 (2013.01); B32B 37/10 (2013.01); C09J 5/02 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C22C 38/06 (2013.01); H02K 1/02 (2013.01); H02K 15/02 (2013.01); B32B 2309/12 (2013.01); B32B 2311/30 (2013.01); C22C 2202/02 (2013.01)] | 10 Claims |

|
1. A bonded and stacked core manufacturing method for manufacturing a bonded and stacked core by performing press working on a strip-shaped steel sheet with a press working oil applied to one surface or both surfaces thereof, applying an adhesive to one surface of the strip-shaped steel sheet and punching out a plurality of steel sheet components, and stacking and bonding the steel sheet components, wherein
a curing accelerator having an average viscosity of 0.01 Pa·s to 100 Pa·s is applied to one surface or both surfaces of the strip-shaped steel sheet before the press working oil is applied.
|