CPC H01M 10/4242 (2013.01) [H01M 10/0525 (2013.01)] | 11 Claims |
1. A method of recovering a degenerated lithium battery cell,
the method comprising:
subjecting a lithium battery cell degenerated by 5% or more to a high temperature treatment for 1 to 6 hours at a temperature within the range of 75° C. to 100° C. in a fully discharged state,
wherein the lithium battery cell comprises an electrode assembly including a positive electrode, a negative electrode and a separator interposed therebetween, which is impregnated with a non-aqueous electrolyte and embedded in a battery case, and
wherein the entire lithium battery cell is maintained at the temperature within the range of 75° C. to 100° C.
|