CPC C04B 38/0006 (2013.01) [B01D 46/0001 (2013.01); B01D 46/2418 (2013.01); B28B 11/006 (2013.01); C04B 14/303 (2013.01); C04B 26/285 (2013.01); C04B 28/24 (2013.01); C04B 38/0012 (2013.01)] | 19 Claims |
1. A method of forming a plugging cement patty, comprising:
mixing a plurality of inorganic particles, an inorganic binder, an organic binder, and a liquid at a mixing temperature greater than a hydration point temperature of the organic binder to form a plugging mixture comprising a viscosity in a range from about 1 cP to about 100 cP;
dispensing the plugging mixture at a dispensing temperature greater than the hydration point temperature; and
cooling the plugging mixture to a cooled temperature less than the hydration point temperature to increase the viscosity of the plugging mixture and form the plugging cement patty.
|