| CPC H01M 4/525 (2013.01) [H01M 4/0416 (2013.01); H01M 4/505 (2013.01); H01M 10/0525 (2013.01)] | 14 Claims |

|
1. A process for producing a coated transition metal oxide, the process comprising:
dry mixing a transition metal oxide and a pyrogenically produced lithium titanate and/or a pyrogenically produced lithium aluminate,
wherein the dry mixing comprises dry mixing 0.05 to 2% by weight of the pyrogenically produced lithium titanate and/or the pyrogenically produced lithium aluminate, wherein the % by weight is relative to a total weight of a mixture of the transition metal oxide and the pyrogenically produced lithium titanate and/or the pyrogenically produced lithium aluminate,
with the transition metal oxide,
to thereby produce the coated transition metal oxide.
|