| CPC B27N 3/002 (2013.01) [B27K 3/20 (2013.01); B27K 3/52 (2013.01); B27N 1/0209 (2013.01); B27N 3/02 (2013.01); C09D 1/02 (2013.01); C09D 197/02 (2013.01); C09K 21/02 (2013.01); B27K 2240/30 (2013.01); B27K 2240/70 (2013.01)] | 5 Claims |
|
1. A fireproof water-resistant wood chip material to make oriented strand boards, comprising a mixture comprising
30 to 43 weight percent of wood chips,
53 to 61.9 weight percent of an aqueous solution of sodium silicate,
2 to 5 weight percent of aluminum hydroxide,
1 to 3 weight percent of water,
0.1 to 1 weight percent of a stabilizer of the aqueous solution of silicate, and
a hardener of the aqueous solution of sodium silicate in the concentration of 0.5 to 5 weight percent to the pure aqueous solution of sodium silicate,
wherein the density of the aqueous solution of sodium silicate ranges from 1370 to 1400 kg/m3, and
wherein the Si02 to Na2O molar ratio in the aqueous solution of sodium silicate ranges from 3.2 to 3.4.
|