| CPC C08G 63/185 (2013.01) [B32B 27/08 (2013.01); B32B 27/34 (2013.01); B32B 27/36 (2013.01); C08L 67/00 (2013.01); C08L 77/00 (2013.01); G02B 1/04 (2013.01); G02B 5/3083 (2013.01); B32B 2250/24 (2013.01); B32B 2307/514 (2013.01); B32B 2307/518 (2013.01); B32B 2307/732 (2013.01); B32B 2457/20 (2013.01); G02F 1/13363 (2013.01); G02F 2413/12 (2013.01); H10K 59/8791 (2023.02)] | 18 Claims |
|
1. A retardation film comprising:
a polyester-series resin exhibiting a negative orientation birefringence and exhibiting a forward wavelength dispersibility in retardation, and
a polyamide-series resin exhibiting a positive orientation birefringence and exhibiting a flat dispersibility in retardation,
wherein the polyester-series resin and the polyamide-series resin have a difference of 0 to 20° C. in glass transition temperature, and
the retardation film is a laminated film comprising: a first layer containing the polyester-series resin, and a second layer containing the polyamide-series resin.
|