CPC H01M 4/134 (2013.01) [H01M 4/045 (2013.01); H01M 4/0452 (2013.01); H01M 4/1395 (2013.01); H01M 4/366 (2013.01); H01M 4/382 (2013.01); H01M 10/052 (2013.01); H01M 2004/021 (2013.01); H01M 2004/027 (2013.01)] | 12 Claims |
1. A lithium metal anode, comprising
a current collector having a flat structure, and
an anode active material layer including a lithium metal disposed on the current collector, and
the lithium metal has a concavo-convex structure,
wherein no dendrite is present on the surface of the lithium metal,
provided that the dendrite refers to a particle in which a ratio of the longest length of the particle in one direction and a length in the direction perpendicular to the longest length of the particle is greater than or equal to 3,
wherein based on a planar projection area of the lithium metal, the lithium metal has pores of 5% to 30% with respect to an entire planar projection area,
wherein a depth of the concavo-convex structure in a thickness direction is 20% to 100% based on total thickness of lithium metal,
wherein a minimum depth of the concavo-convex structure in a thickness direction is 20% to 50%, and
wherein a maximum depth of the concavo-convex structure in a thickness direction is 100%.
|