CPC B32B 15/046 (2013.01) [B32B 5/18 (2013.01); B32B 15/20 (2013.01); C09D 107/00 (2013.01); C09D 109/06 (2013.01); C09D 111/00 (2013.01); C09D 127/06 (2013.01); C09D 127/08 (2013.01); C09D 133/08 (2013.01); C09D 163/00 (2013.01); C09D 175/02 (2013.01); C09D 175/04 (2013.01); C09D 183/06 (2013.01); C09D 195/005 (2013.01); E04B 1/665 (2013.01); E04C 2/26 (2013.01); B32B 2255/102 (2013.01); B32B 2255/26 (2013.01); B32B 2266/0214 (2013.01); B32B 2307/304 (2013.01); B32B 2307/7242 (2013.01); B32B 2307/7246 (2013.01); B32B 2419/00 (2013.01); E04B 2103/02 (2013.01); E04B 2103/04 (2013.01)] | 23 Claims |
1. An integrated air barrier assembly comprising:
a board including a first surface and a second surface;
a fastener-sealing layer comprising a liquid-applied coating composition adhered on one of the first surface or the second surface of the board, wherein the fastener-sealing layer has a glass transition temperature of equal to or less than 40° F. such that the fastener-sealing layer is soft enough to seal around a shaft of a fastener and has a thickness ranging from 1 mils to 50 mils, wherein the liquid-applied coating composition comprises at least one of a liquid-applied latex, acrylic, vinyl acrylic, styrene acrylate, vinyl acetate, styrene-butadiene, carboxylated styrene-butadiene, vinylidene chloride, asphaltic emulsion, natural rubber, butyl, chloroprene, vinyl chloride-ethylene, and polyvinyl chloride; and
an anti-blocking facing layer adhered on a surface of the fastener-sealing layer opposite the board such that the fastener-sealing layer is disposed between the board and the anti-blocking facing layer, wherein the anti-blocking facing layer is chosen from a fiberglass mat, an aluminum foil, a fabric layer, or a paper layer, or a combination thereof,
wherein the assembly has an air leakage of less than 0.02 L/sec-m2 as measured by ASTM Test Method E 2178 (2003) at a pressure difference of 75 Pa.
|