US 12,460,111 B2
Reinforcing fibers and production method therefor, and molded article using same
Toru Asada, Okayama (JP); Daisuke Koda, Kamisu (JP); Shinichi Takemoto, Okayama (JP); Hiroyuki Kawai, Okayama (JP); and Shuhei Yorimitsu, Okayama (JP)
Assigned to KURARAY CO., LTD., Kurashiki (JP)
Appl. No. 17/059,103
Filed by KURARAY CO., LTD., Kurashiki (JP)
PCT Filed May 28, 2019, PCT No. PCT/JP2019/021036
§ 371(c)(1), (2) Date Nov. 25, 2020,
PCT Pub. No. WO2019/230700, PCT Pub. Date Dec. 5, 2019.
Claims priority of application No. 2018-102577 (JP), filed on May 29, 2018.
Prior Publication US 2021/0222036 A1, Jul. 22, 2021
Int. Cl. C09J 109/00 (2006.01); B60C 9/00 (2006.01); C08J 5/06 (2006.01); C08L 9/00 (2006.01)
CPC C09J 109/00 (2013.01) [C08J 5/06 (2013.01); C08L 9/00 (2013.01); B60C 9/0042 (2013.01); B60C 2009/0071 (2013.01); C08J 2309/00 (2013.01); C08J 2467/00 (2013.01); C08L 2205/03 (2013.01); C08L 2205/16 (2013.01)] 20 Claims
 
1. Reinforcing fibers, comprising:
hydrophilic fibers and
an adhesive component,
wherein:
surfaces of the hydrophilic fibers are at least partially covered with the adhesive component,
the adhesive component comprises a modified conjugated diene rubber having a hydrogen-bonding functional group in a part of the modified conjugated diene rubber, and an emulsifier,
the number of the hydrogen-bonding functional groups in the modified conjugated diene rubber is from 2 to 150 per molecule on average,
a melt viscosity measured at 38° C. of the modified conjugated diene rubber is from 0.1 to 4,000 Pa·s, and
the number-average molecular weight (Mn) of the modified conjugated diene rubber is at least 20,000.