| CPC C08F 220/22 (2013.01) [C08F 2/50 (2013.01); C08F 2/54 (2013.01); C08F 14/18 (2013.01); C08L 27/12 (2013.01)] | 4 Claims |
|
1. A method of producing a fluororesin cured product, comprising:
baking a photosensitive resin composition at a temperature of 140° C. or lower for curing to form a fluororesin cured product, wherein the photosensitive resin composition comprises:
a fluororesin having a crosslinking site;
a solvent; and
a photopolymerization initiator,
wherein the fluororesin contains a repeating unit derived from a hydrocarbon having a fluorine atom, and
wherein the repeating unit derived from a hydrocarbon having a fluorine atom has a structure represented by the following formula (1-1);
![]() wherein each Rf independently represents a fluorine atom or a perfluoroalkyl group selected from a C1-C6 linear, C3-C6 branched, or C3-C6 cyclic perfluoroalkyl group; and R1-2 represents a hydrogen atom or an alkyl group selected from a C1-C6 linear, C3-C6 branched, or C3-C6 cyclic alkyl group.
|