CPC G02B 1/11 (2013.01) [G02F 1/133502 (2013.01); G06F 3/041 (2013.01)] | 10 Claims |
1. An anti-glare film comprising an anti-glare layer, wherein
the anti-glare layer has a 500-μm square area, as measured for surface roughness, satisfying condition 1 and condition 2 below, where the maximum peak height is defined as P, a plane having a height obtained by adding P/6 to the average height is defined as a first reference plane, the number of projections exceeding the first reference plane is defined as N1, a plane having a height obtained by adding P/3 to the average height is defined as a second reference plane, and the number of projections exceeding the second reference plane is defined as N2:
P is 0.20 μm or more and 1.20 μm or less; and <condition 1>
0.20≤N2/N1≤0.45. <condition 2>.
|