CPC D01D 4/02 (2013.01) [D01D 10/02 (2013.01); D01F 2/06 (2013.01); D01F 2/00 (2013.01)] | 10 Claims |
1. A method of producing lyocell filaments; employing a steam heatable spinneret having a rectangular shape with an aspect ratio of more than 2 and comprising at least a top housing and a nozzle frame, the method comprising:
preparing a spinning solution and extruding the spinning solution with the steam heatable spinneret,
wherein the top housing or the top housing and the nozzle frame is heated by steam having a temperature ranging from 105 to 138° C. and a pressure ranging from 1.2 to 4 bar.
|