| CPC C04B 28/105 (2013.01) [C04B 9/20 (2013.01); C04B 22/16 (2013.01); C04B 24/06 (2013.01); C04B 24/10 (2013.01); C04B 24/2623 (2013.01); C04B 24/34 (2013.01); C04B 38/10 (2013.01); C04B 2103/12 (2013.01); C04B 2103/22 (2013.01); C04B 2103/302 (2013.01); C04B 2103/304 (2013.01)] | 17 Claims |
|
1. A method of producing magnesium cement,
the method comprising:
mixing:
water at a temperature of between approximately 50° C. and 100° C., wherein the water comprises total dissolved solids of greater than 0 g/L and less than approximately 350 g/L;
a magnesium oxygen-containing compound; and
a magnesium salt; and
increasing the amount of the total dissolved solids in the water before the mixing step.
|