| CPC B05D 3/068 (2013.01) [B05D 3/0254 (2013.01); B05D 2202/00 (2013.01); B05D 2203/35 (2013.01); B05D 2503/00 (2013.01); C09D 11/30 (2013.01); C09D 175/04 (2013.01)] | 20 Claims |
|
1. Method of coating a substrate comprising the steps of:
applying to the substrate from 0.1 to 250 g/m2m2 (dry matter) of a radiation curable aqueous composition comprising from 15 to 50 wt % of a dispersed polymeric binder and from 0 to 15 wt % of an unsaturated reactive diluent;
thermally drying the aqueous composition to form a dust-free film; and
electron beam curing the thermally dried composition,
the method being characterized by the fact that the dispersed polymeric binder is a polyurethane binder, the aqueous coating composition is a physically drying, film-forming aqueous composition containing from 100 to 600 meq/100 g (dry matter) of radiation curable unsaturated groups and that the curing is performed in air atmosphere.
|