| CPC C09K 5/14 (2013.01) [B22F 1/05 (2022.01); B22F 3/105 (2013.01); B22F 3/14 (2013.01); B22F 2003/1051 (2013.01); B22F 2301/10 (2013.01); B22F 2302/406 (2013.01); B22F 2304/10 (2013.01)] | 20 Claims |

|
1. A method of producing a composite material, the method comprising:
preparing a mixed powder of diamond particles and copper powder particles; and
generating a composite material containing diamond and copper from the mixed powder by pulsed electric current sintering with repeated application of a first pressure and a second pressure higher than the first pressure, each of the first pressure and the second pressure being 5 MPa or greater and 100 MPa or less applied to the mixed powder, and with the mixed powder maintained at a temperature equal to or higher than 500° C. and lower than 800° C.
|