| CPC B01D 61/026 (2022.08) [B01D 67/0002 (2013.01); B01D 67/00931 (2022.08); B01D 71/56 (2013.01); B82Y 30/00 (2013.01); B82Y 40/00 (2013.01); C02F 1/265 (2013.01); B01D 2323/21819 (2022.08); C02F 2103/08 (2013.01)] | 5 Claims |

|
1. A process for obtaining polyamide membrane with nanostructured coating, the process comprising the following steps:
(a) prepare dispersion of graphene oxide (GO) in absolute ethyl alcohol (99.5%) between 0.1 g/L and 2 g/L;
(b) apply the dispersion obtained in step (a) on reverse osmosis membranes made of a selective polyamide (PA) layer, using spin coating technique, with low rotation stage followed by high rotation;
(c) repeat step (b) between 1 and 5 times; and
(d) immerse the membranes in water immediately after step (c).
|