CPC C04B 26/16 (2013.01) [C04B 14/06 (2013.01); C04B 14/28 (2013.01); C04B 18/142 (2013.01); C04B 20/1003 (2013.01); C04B 28/082 (2013.01); C04B 2103/30 (2013.01); C04B 2103/408 (2013.01); C04B 2111/00482 (2013.01); C04B 2111/00637 (2013.01); C04B 2111/00689 (2013.01); C04B 2111/60 (2013.01); C04B 2111/70 (2013.01); C04B 2111/94 (2013.01)] | 10 Claims |
1. A method comprising
a step of grouting of machines or turbines with a curable binder composition comprising: a) at least one organic binder selected from the group consisting of a1) epoxy resins and curing agents for epoxy resins and a2) polyisocyanates and polyols, and b) at least 50% by weight of slag based on 100% by weight of the binder composition,
wherein the slag has a bulk density of at least 2.9 kg/l, and
wherein the slag is an iron-containing slag containing at least 8% by weight, of iron, calculated as FeO.
|