| CPC C21D 6/008 (2013.01) [C21D 9/46 (2013.01); C22C 38/02 (2013.01); C22C 38/04 (2013.01); C21D 2201/05 (2013.01)] | 14 Claims |
|
1. A grain oriented electrical steel sheet comprising: a steel sheet; and a coating disposed on each of both surfaces of the steel sheet,
wherein an interlaminar current value after a rubbing test is not more than 0.10 A,
the rubbing test being conducted by stacking two sheets of the grain oriented electrical steel sheet and rubbing the two sheets against each other to make 90 reciprocations under conditions of a surface pressure of 200 Pa, a rubbing speed of 0.10 m/s, and a reciprocating stroke of 50 mm.
|