| CPC C10G 67/02 (2013.01) [B01D 17/06 (2013.01); B01J 27/051 (2013.01); C10G 1/10 (2013.01); C10G 2300/1003 (2013.01); C10G 2300/4012 (2013.01)] | 19 Claims |

|
1. A method for refining waste plastic pyrolysis oil, the method comprising the steps of:
S1) mixing waste plastic pyrolysis oil, washing water, and a demulsifier to form a first mixed solution and dehydrating the first mixed solution by applying a voltage to form a dehydrated first mixed solution; and
S2) mixing the dehydrated first mixed solution and a sulfur source to obtain a second mixed solution and hydrotreating the second mixed solution to produce a stream comprising a refined oil from which sulfur and nitrogen impurities have been removed.
|