| CPC C08K 9/06 (2013.01) [C09C 3/12 (2013.01); C01P 2004/64 (2013.01); C01P 2006/12 (2013.01); C08K 2201/006 (2013.01); C08K 2201/011 (2013.01)] | 10 Claims |
|
1. A ZrO2 dispersion liquid comprising: a Zro2 particle coated with a silane coupling agent, and a dispersion medium for the ZrO2 particle, wherein a BET specific surface area of the ZrO2 particle coated with the silane coupling agent obtained by removing the dispersion medium is 36% or more of a BET specific surface area of the Zro2 particle before coating with the silane coupling agent, and an average primary particle size of the ZrO2, particle before coating with the silane coupling agent is 3.0 nm or more and 20.0 nm or less.
|