| CPC B65D 65/40 (2013.01) [B32B 7/03 (2019.01); B32B 27/08 (2013.01); B32B 27/18 (2013.01); B32B 27/306 (2013.01); B32B 27/32 (2013.01); B32B 33/00 (2013.01); B32B 2250/02 (2013.01); B32B 2250/24 (2013.01); B32B 2307/72 (2013.01); B32B 2311/24 (2013.01); B65D 75/322 (2013.01); B65D 75/5877 (2013.01); B65D 2565/385 (2013.01)] | 20 Claims |

|
1. A recyclable bag having a metallized barrier co-extruded multi-layer polymeric film comprising:
(i) an inner sealant layer comprising an ethylene/α-olefin interpolymer fraction having a density in the range of 0.894 to 0.924 g/cm3 in an amount of at least about 40-50% by weight or thickness of the total inner sealant layer;
(ii) a core barrier layer comprising ethylene-vinyl alcohol (EVOH) comprising about 0.1% to about 10% by total weight or thickness of the metallized barrier co-extruded multi-layer polymeric film, wherein the EVOH comprises from about 27-55 mol % ethylene in the EVOH copolymer; and
(iii) an outer metallized sealant layer comprising a polyethylene polymer, a polyethylene copolymer, or an ethylene/a-olefin interpolymer, having a density in the range of 0.894 to 0.935 g/cm3, in an amount of at least about 40-50% by weight or thickness of the total outer metallized sealant layer, and a material that increases metal adhesion.
|