CPC H01M 4/5825 (2013.01) [C01B 25/45 (2013.01); H01M 4/131 (2013.01); H01M 10/052 (2013.01); C01P 2002/54 (2013.01); C01P 2002/60 (2013.01); C01P 2002/72 (2013.01); C01P 2006/40 (2013.01); H01M 2004/021 (2013.01); H01M 2004/028 (2013.01)] | 12 Claims |
1. A cathode active material for a lithium secondary battery comprising a lithium metal phosphate particle having a crystallite size in a range from 150 nm to 450 nm in a direction of a crystallographic plane (020) as measured by an X-ray diffraction (XRD) analysis,
wherein a particle crystallite size ratio determined by Equation 2 based on a measurement by the XRD analysis is greater than 0 and less than 1:
particle crystallite size ratio=Lp(020)/Lp(200) [Equation 2]
wherein, in Equation 2, Lp(020) is a value in nm corresponding to the crystallite size in the direction of the crystallographic plane (020) of the lithium metal phosphate particle, and Lp(200) is a value in nm corresponding to a crystallite size in a direction of a crystallographic plane (020) of the lithium metal phosphate particle.
|