| CPC H01M 4/362 (2013.01) [C01B 32/21 (2017.08); C01B 33/02 (2013.01); H01M 4/0433 (2013.01); H01M 4/0471 (2013.01); H01M 4/133 (2013.01); H01M 4/134 (2013.01); H01M 4/386 (2013.01); H01M 4/587 (2013.01); H01M 10/0525 (2013.01); H01M 2004/027 (2013.01)] | 11 Claims |

|
1. A method of preparing an anode active material for a lithium secondary battery, comprising:
preparing a porous silicon-carbon mixed powder by mixing nano-silicon particles, graphite particles, and pitch particles by dry milling;
adding the porous silicon-carbon mixed powder and a binder to distilled water to prepare a mixed solution;
spray-drying the mixed solution to prepare primary particles;
inserting the primary particles into a mold and press-molding to produce secondary particles;
heat-treating the secondary particles to produce heat-treated secondary particles; and
pulverizing and sieving the heat-treated secondary particles,
wherein, in the preparing of the porous silicon-carbon mixed powder, the pitch particles are included in an amount of greater than or equal to 30 wt % based on 100 wt % of the porous silicon-carbon mixed powder.
|