| CPC C10M 125/22 (2013.01) [C01G 39/06 (2013.01); C10M 139/00 (2013.01); C10M 141/12 (2013.01); C10M 169/04 (2013.01); C01P 2002/60 (2013.01); C01P 2002/72 (2013.01); C01P 2002/74 (2013.01); C01P 2002/76 (2013.01); C01P 2004/61 (2013.01); C01P 2004/62 (2013.01); C01P 2004/64 (2013.01); C01P 2006/12 (2013.01); C10M 2201/066 (2013.01); C10M 2203/003 (2013.01); C10N 2020/06 (2013.01)] | 14 Claims |

|
1. Molybdenum disulfide particles comprising:
a 2H crystal structure and a 3R crystal structure of molybdenum disulfide, wherein
a presence ratio of the 3R crystal structure in a crystal phase of molybdenum disulfide is 10% or more, and
a crystallite size of the 3R crystal structure calculated by extended-type Rietveld analysis based on an analysis formula L=Kλ/(βcosθ) using a profile obtained from powder X-ray diffraction (XRD) using Cu-Kα rays as an X-ray source is 1 nm to 150 nm,
(in the above formula, K is an instrumental constant that depends on an XRD optical system (an incident side and a detector side) and settings, L is a crystallite size [m], λ is a measured X-ray wavelength [m], β is a half width [rad], and θ is a Bragg angle of a diffraction line [rad]).
|