| CPC C09C 1/0003 (2013.01) [C09C 3/06 (2013.01); C23C 16/342 (2013.01); C23C 16/4417 (2013.01); H01B 3/02 (2013.01); C01P 2004/03 (2013.01); C01P 2004/04 (2013.01); C01P 2004/13 (2013.01); C01P 2006/40 (2013.01)] | 13 Claims |

|
1. A method of making an encapsulated nanoribbon comprising:
reacting an encapsulated first precursor with a second precursor to provide an encapsulated nanoribbon, wherein reacting the encapsulated first precursor with the second precursor comprises contacting the encapsulated first precursor with a vapor of the second precursor at an elevated temperature for a time period sufficient to provide the encapsulated nanoribbon.
|