| CPC C08G 63/183 (2013.01) [C08J 5/18 (2013.01); C09D 167/02 (2013.01); C08J 2367/02 (2013.01)] | 7 Claims |

|
1. A manufacturing method of a polyester for a plastic wrap, comprising:
providing an aromatic carboxylic acid, an aliphatic carboxylic acid and an aliphatic alcohol, wherein the aromatic carboxylic acid comprises at least two from the group consisting of a phthalic acid, an isophthalic acid, and a terephthalic acid; and
obtaining a polybutylene adipate terephthalate by subjecting the aromatic carboxylic acid, the aliphatic carboxylic acid, and the aliphatic alcohol to at least an esterification reaction, a pre-polymerization reaction and a polymerization reaction in sequence,
wherein in the polybutylene adipate terephthalate, a ratio of a number of moles of the aromatic carboxylic acid to a number of moles of the aliphatic carboxylic acid ranges from 0.55:0.45 to 0.2:0.8, and the polybutylene adipate terephthalate accounts for more than 95 wt % of the plastic wrap.
|