| CPC C08G 59/245 (2013.01) [C08J 3/24 (2013.01); C08J 2363/02 (2013.01)] | 7 Claims |

|
1. An environment-friendly vinyl ester resin prepared by mixing following raw materials in percentage by weight: 20-65 weight percentage (wt %) of epoxy resin, 5-35 wt % of methyl monomer, 8-25 wt % of unsaturated acid, 0.01-0.3 wt % of a catalyst, 0.01-0.08 wt % of polymerization inhibitor and 10-40 wt % of a cross-linking agent;
wherein the catalyst is prepared by mixing following raw materials in percentage by weight: 5-20 wt % of cobalt chloride, 10-30 wt % of sodium hydroxide, 20-60 wt % of acetylacetone and 10-40 wt % of water.
|