| CPC C02F 1/46109 (2013.01) [C02F 2001/46138 (2013.01); C02F 2001/46161 (2013.01)] | 12 Claims |

|
1. A method to prepare a graphene coated sponge-based electrode comprising:
obtaining a graphene coated sponge by:
filling mineral wool with a solution comprising graphene material by successive squeezing to obtain a mineral wool soaked with graphene material;
transferring the mineral wool soaked with graphene material into a hydrothermal reactor and submitting it to heating from 60 to 240° C. for 5 minutes to 72 hours to have graphene material bonded to mineral wool;
cleaning the heated material to remove the unbonded graphene material and reaction by-products from the graphene coated mineral wool; and
connecting the graphene coated sponge to electrical current.
|