CPC C09D 127/18 (2013.01) [C09D 175/04 (2013.01)] | 4 Claims |
1. A mixed coating material, consisting of:
a cold curing resin that undergoes reaction curing at normal room temperature; and
a tetrafluoroethylene resin including particulate bodies and having an average molecular weight ranging from 500 to 5000,
wherein a constituent ratio of the tetrafluoroethylene resin in a coating film that is a cured state of the mixed coating material ranges from 55 wt % to 67.3 wt %, and
wherein the cold curing resin is a polyurethane resin.
|