CPC C08G 65/34 (2013.01) [B01J 31/0225 (2013.01); B01J 31/0251 (2013.01); B01J 31/0298 (2013.01)] | 19 Claims |
1. A method for preparing a polyether, comprising the steps of:
a) mixing at least one optionally substituted and optionally polymeric alcohol comprising at least two terminal hydroxyl groups with a protic ionic salt formed by the combination of a Brønsted acid and a Brønsted base, wherein the molar proportion of the protic ionic salt with respect to the total amount of moles of the alcohol is between 1 to 15%;
b) heating the mixture obtained in step (a) at a temperature comprised between 100° C. and 300° C.
|