CPC C08L 53/02 (2013.01) [C08L 23/12 (2013.01); C08L 23/16 (2013.01); C08L 2205/03 (2013.01)] | 15 Claims |
1. A thermoplastic elastomer comprising a styrene block copolymer and a non-elastomeric polyolefin, wherein the non-elastomeric polyolefin has a melt flow rate MFR of more than 5 dg/min, a crystallization endset temperature Tcendset of equal to or less than 110° C., and a crystallization onset temperature Tconset in the range of more than 100° C. and less than 130° C., with the proviso that the crystallization endset temperature Tcendset is smaller than the crystallization onset temperature Tconset.
|