| CPC H01M 4/0459 (2013.01) [H01M 4/0445 (2013.01); H01M 10/0525 (2013.01); H01M 2004/027 (2013.01)] | 11 Claims |

|
1. A method for pre-lithiation of a negative electrode comprising:
interposing a separator between a lithium ion-supplying metal sheet and a negative electrode to prepare a simple cell;
immersing the simple cell in an electrolyte for pre-lithiation; and
disposing the simple cell immersed in the electrolyte for pre-lithiation between two polymer pads, and carrying out electrochemical charging, while pressurizing the outside of the two polymer pads by using a pressurizing member provided with a pair of jigs, to perform pre-lithiation of the negative electrode,
wherein each of the polymer pads has a thickness of 60% to 90% of a thickness of a corresponding jig of the pair of jigs,
wherein the pressurizing is conducted under a pressure of 0.01-10 kPa.
|