| CPC C08K 3/34 (2013.01) [C01B 33/24 (2013.01); C08K 7/10 (2013.01)] | 12 Claims |

|
1. A fibrous wollastonite in which Al, Fe, and Si are detected by surface analysis by time-of-flight secondary ion mass spectrometry, with a detection intensity ratio of Fe to Si being less than 0.13, a detection intensity ratio of Al to Fe being 5 or more and 50 or less, and a detection intensity ratio of Al to Si being greater than 0.03 to less than 1.08,
wherein Al and Fe are impurities, and
wherein an average fiber length of the fibrous wollastonite is in a range of 3 μm to 100 μm.
|