| CPC C09D 7/65 (2018.01) [C08K 3/22 (2013.01); C08L 5/08 (2013.01); C09D 5/022 (2013.01); C09D 5/025 (2013.01); C09D 5/028 (2013.01); C09D 7/20 (2018.01); C09D 7/61 (2018.01); C09D 7/69 (2018.01); C09D 7/80 (2018.01); C09D 105/08 (2013.01); C09D 133/04 (2013.01); C08K 2003/2241 (2013.01)] | 16 Claims |

|
1. A method of making a coating composition comprising:
blending a binder, a surfactant, and a first aqueous carrier to form a pre-thin:
adding an aqueous solution of chitosan having a number average molecular weight of at most 40,000 or a weight average molecular weight of at most 75,000 or a z-average molecular weight of at most 200,000 and having a pH of less than 6.5, a pigment and a second aqueous carrier liquid, optional additives, and a base to precipitate the chitosan into precipitated chitosan;
grinding, in grind stage, the pigment with the second aqueous carrier liquid, precipitated chitosan and optional additives, to disperse the pigment, precipitated chitosan, and optional additives into a grind paste;
adding, in a wash stage using a wash liquid, the grind paste to the pre-thin;
blending, in a thindown stage, the grind paste and the pre-thin to form a coating composition having a pH of about 8 to about 10.
|