| CPC C01B 25/321 (2013.01) [C08K 3/32 (2013.01); C09D 5/084 (2013.01); C08K 2003/321 (2013.01); C08K 2201/006 (2013.01)] | 14 Claims |
|
1. A method for producing a phosphate-containing anti-corrosion pigment, comprising the following steps:
a) providing hydroxyapatite or calcium-magnesium-phosphate particles or mixtures of the aforementioned as start particles in an aqueous solvent or dispersant,
b) adding lime milk, a magnesium compound, and phosphoric acid to the aqueous solvent or dispersant in order to produce a reaction mixture,
c) reacting the reaction mixture to form the phosphate-containing anti-corrosion pigment:
at a temperature in the range of 20° C. to 105° C. and
at a pH value in the range of 6.0 to 13.0,
d) separating at least a part of the phosphate-containing anti-corrosion pigment from the aqueous solvent or dispersant, and
e) Optionally: drying the phosphate-containing anti-corrosion pigment.
|