CPC H01M 4/1393 (2013.01) [H01M 4/04 (2013.01); H01M 4/133 (2013.01); H01M 4/134 (2013.01); H01M 4/1395 (2013.01); H01M 4/364 (2013.01); H01M 4/386 (2013.01); H01M 4/583 (2013.01); H01M 10/052 (2013.01); H01M 10/0525 (2013.01); H01M 2004/021 (2013.01); H01M 2004/027 (2013.01); Y02T 10/70 (2013.01)] | 16 Claims |
1. A method of making a silicon-carbon particulate composite, comprising co-milling silicon and carbonaceous starting materials under wet conditions to produce a silicon-carbon particulate composite having a nanostructure which inhibits or prevents silicon pulverization when used as active material in a negative electrode of a Li-ion battery and/or which maintains electrochemical capacity of a negative electrode;
wherein the carbonaceous starting material is selected from a natural graphite, a synthetic graphite, or a mixture of natural and synthetic graphite; wherein the natural or synthetic graphite is exfoliated graphite or expanded graphite.
|