CPC C08L 95/00 (2013.01) [C04B 24/02 (2013.01); C04B 26/26 (2013.01); C08K 5/05 (2013.01); C08L 91/00 (2013.01); C08L 95/005 (2013.01); E01C 7/353 (2013.01); E01C 11/005 (2013.01); C04B 2111/00612 (2013.01); C04B 2111/0075 (2013.01); C08L 2207/22 (2013.01); C08L 2555/28 (2013.01); C08L 2555/34 (2013.01); C08L 2555/60 (2013.01); Y02W 30/91 (2015.05)] | 13 Claims |
1. A method of road paving comprising:
providing sterol-containing asphalt binder emulsion, wherein sterol is added to an asphalt binder from 0.5 to 15 wt. % of the sterol based on the asphalt binder before emulsification;
combining the sterol-containing asphalt binder emulsion with aggregate to form an asphalt paving material;
applying the asphalt paving material atop an asphalt pavement layer; and
compacting the applied asphalt paving material to form a road pavement having a sterol-containing topcoat layer.
|