CPC C08L 23/12 (2013.01) [C08L 2203/18 (2013.01); C08L 2205/03 (2013.01); C08L 2207/02 (2013.01); C08L 2207/10 (2013.01); C08L 2207/20 (2013.01)] | 16 Claims |
1. A composition comprising a recycled polymer composition (RPC) and a heterophasic propylene copolymer (HECO), the composition is obtained by blending,
wherein
(a) the recycled polymer composition (RPC) comprises at least 80 wt.-%, based on the weight of the recycled polymer composition (RPC), of a recycled polypropylene, and
(b) the heterophasic propylene copolymer (HECO) has
(b1) a xylene cold soluble (XCS) fraction determined at 25° C. according to ISO 16152 in the range of 5.0 to 18 wt.-%, and
(b2) a melt flow rate MFR2 (230° C./2.16 kg) measured according to ISO 1133 in the range of 0.05 to 1.5 g/10 min,
wherein further
(a) the weight ratio between the heterophasic propylene copolymer (HECO) and the recycled polymer composition (RPC) [(HECO)/(RPC)] is in the range of 1.1 to 7.0,
(b) the percentage by weight of the heterophasic propylene copolymer (HECO) together with the recycled polymer composition (RPC) [(HECO)+(RPC)], based on the weight of the composition, is at least 85 wt.-%, and
(c) the composition has a tensile modulus measured according to ISO 527-2 in the range of 1100 to 1600 MPa and/or a content of limonene as determined using solid phase microextraction (HS-SPME-GC-MS) of from 0.5 to 40 mg/kg.
|