CPC C09D 177/04 (2013.01) [B05D 7/00 (2013.01); B05D 7/24 (2013.01); B32B 27/18 (2013.01); B32B 27/40 (2013.01); C08G 18/022 (2013.01); C08G 18/092 (2013.01); C08G 18/10 (2013.01); C08G 18/32 (2013.01); C08G 18/4277 (2013.01); C08G 18/73 (2013.01); C08G 18/7837 (2013.01); C08G 18/79 (2013.01); C08G 18/792 (2013.01); C09D 5/08 (2013.01); C09D 175/04 (2013.01); C09D 175/06 (2013.01)] | 17 Claims |
1. A method for preventing corrosion of a structure, comprising:
coating the structure with a polyaspartic coating composition, comprising:
(A) an aspartic acid ester compound represented by the following formula (I)
![]() wherein X is an n-valent organic group obtained by removing a primary amino group of an n-valent polyamine, and R1 and R2 are the same or different organic groups which are inert to the isocyanate group under a reaction condition, and n is an integer of 2 or more, and
(B) a polyisocyanate component obtained by reacting one or two or more diisocyanate monomers selected from the group consisting of an aliphatic and alicyclic diisocyanate with a polycaprolactone polyol having a number-average molecular weight of 500 to 1,500,
wherein
a ratio of the polycaprolactone polyol to a total amount of the polyol is 20% by mass or more,
the polyisocyanate component contains 10.0% by mass or less of an isocyanurate trimer with respect to a total amount of the polyisocyanate component,
the structure is a bridge, a highway, a power transmission tower, or a wind power generation blade, and
the polyol further contains a polyoxyalkylene polyol.
|