US 12,733,198 B2
Semiconductor device and method of manufacture
Li-Li Su, ChuBei City (TW); Wei-Min Liu, Hsinchu (TW); Wei Hao Lu, Taoyuan City (TW); Chien-I Kuo, Zhubei City (TW); and Yee-Chia Yeo, Hsinchu (TW)
Assigned to Taiwan Semiconductor Manufacturing Co., Ltd., Hsinchu (TW)
Filed by Taiwan Semiconductor Manufacturing Co., Ltd., Hsinchu (TW)
Filed on Jul. 20, 2022, as Appl. No. 17/813,866.
Application 17/813,866 is a division of application No. 16/941,427, filed on Jul. 28, 2020, granted, now 11,532,750.
Claims priority of provisional application 62/982,427, filed on Feb. 27, 2020.
Prior Publication US 2022/0367717 A1, Nov. 17, 2022
Int. Cl. H10D 30/62 (2025.01); H10D 30/01 (2025.01); H10D 84/01 (2026.01); H10D 84/03 (2025.01)
CPC H10D 30/6211 (2025.01) [H10D 30/0241 (2025.01); H10D 84/0147 (2025.01); H10D 84/0158 (2025.01); H10D 84/038 (2025.01)] 20 Claims
OG exemplary drawing
 
1. A method comprising:
depositing a dummy gate over and along sidewalls of a fin extending upwards from a substrate;
forming a gate spacer along a sidewall of the dummy gate;
forming a recess in the fin adjacent the gate spacer; and
forming a source/drain region in the recess, the forming of the source/drain region comprising:
epitaxially growing a first doped silicon layer lining the recess, wherein the first doped silicon layer is doped with arsenic, wherein portions of the first doped silicon layer near a top of the recess have a first thickness, wherein portions of the first doped silicon layer near a bottom of the recess have a second thickness that is greater than the first thickness; and
epitaxially growing a second doped silicon layer on the first doped silicon layer, wherein the second doped silicon layer is doped with phosphorus, and wherein the source/drain region has a doping transition length in a range of 7 nm to 15 nm, wherein the doping transition length is defined as a distance from an interface between the source/drain region and a channel region to a position in the channel region at which a total dopant concentration is less than 1E1018 atoms/cm3.
 
8. A method comprising:
etching a recess in a semiconductor fin, wherein the recess is adjacent a channel region of the semiconductor fin; and
forming a source/drain region in the recess and having a doping transition length in a range of 7 nm to 15 nm, wherein the doping transition length is defined as a distance from an interface between the source/drain region and the channel region to a position in the channel region at which a total dopant concentration is less than 1E1018 atoms/cm3, wherein forming the source/drain region comprises:
performing a first epitaxial growth process to form a first epitaxial layer on surfaces of the recess, wherein the first epitaxial layer comprises a first n-type dopant, wherein the first epitaxial layer has a region of maximum concentration of the first n-type dopant that is separated from upper surfaces of the first epitaxial layer by a nonzero first distance;
performing a second epitaxial growth process to form a second epitaxial layer on the first epitaxial layer, wherein the second epitaxial layer comprises a second n-type dopant that has a larger diffusivity than the first n-type dopant, the second epitaxial growth process does not use any precursor that comprises the first n-type dopant to form the second epitaxial layer; and
after performing the second epitaxial growth process, diffusing the first n-type dopant from the first epitaxial layer into the second epitaxial layer.
 
15. A method comprising:
forming a fin protruding from a semiconductor substrate;
forming a source/drain region in the fin, comprising:
forming a recess in the fin, wherein the recess is U-shaped;
forming a conformal layer of arsenic-doped silicon in the recess, wherein the conformal layer of arsenic-doped silicon has a thickness in a range of 1 nm to 12 nm; and
filling remaining portions of the recess with phosphorus-doped silicon, wherein the maximum concentration of phosphorus in the phosphorus-doped silicon is greater than the maximum concentration of arsenic in the conformal layer of arsenic doped silicon, wherein the phosphorus-doped silicon comprises arsenic, and wherein a concentration of phosphorus in the phosphorus-doped silicon is greater than a concentration of arsenic in the phosphorus-doped silicon; and
forming a contact plug protruding into the phosphorus-doped silicon, wherein the contact plug is separated from the conformal layer of arsenic-doped silicon, wherein the source/drain region has a doping transition length in a range of 7 nm to 15 nm, and wherein the doping transition length is defined as a distance from an interface between the source/drain region and a channel region to a position in the channel region at which a total dopant concentration is less than 1E1018 atoms/cm3.