US 12,731,786 B2
Lithium metal composite oxide, positive electrode active substance for lithium secondary battery, positive electrode for lithium secondary battery, lithium secondary battery, and method for producing lithium metal composite oxide
Tomoya Kuroda, Fukui (JP); and Yuichi Sato, Niihama (JP)
Assigned to Sumitomo Metal Mining Co., Ltd., Tokyo (JP)
Appl. No. 17/791,161
Filed by Sumitomo Metal Mining Co., Ltd., Tokyo (JP)
PCT Filed Jan. 8, 2021, PCT No. PCT/JP2021/000492
§ 371(c)(1), (2) Date Jul. 6, 2022,
PCT Pub. No. WO2021/141112, PCT Pub. Date Jul. 15, 2021.
Claims priority of application No. 2020-002395 (JP), filed on Jan. 9, 2020.
Prior Publication US 2023/0039190 A1, Feb. 9, 2023
Int. Cl. H01M 4/525 (2010.01); H01M 4/02 (2006.01); H01M 4/04 (2006.01); H01M 4/505 (2010.01); H01M 10/0525 (2010.01)
CPC H01M 4/525 (2013.01) [H01M 4/043 (2013.01); H01M 4/0471 (2013.01); H01M 4/505 (2013.01); H01M 10/0525 (2013.01); H01M 2004/021 (2013.01); H01M 2004/028 (2013.01)] 18 Claims
OG exemplary drawing
 
1. A lithium metal composite oxide having a layered structure, comprising at least lithium, nickel, and an element X, wherein:
the lithium metal composite oxide is represented by composition formula (A):
Li[Lim(Ni(1-n)Xn)1-m]O2  (A),
wherein m and n satisfy −0.1≤m≤0.2, 0<n≤0.6 and 0<m+n<0.6,
the element X is at least one element selected from the group consisting of Co, Mn, Fe, Cu, Ti, Mg, Al, W, Mo, Nb, Zn, Sn, Zr, Ga, V, B, Si, S and P,
the lithium metal composite oxide contains single particles and satisfies all of requirements (1) to (5):
(1): a volume-based 50% cumulative particle size D50 of the lithium metal composite oxide is 2 μm or more and 10 μm or less;
(2): the single particles have, on at least a part of surfaces thereof, adhered fine particles, with the proviso that a maximum particle size of the adhered fine particles is smaller than a particle size of the single particles;
(3): the particle size of the single particles is 0.2 to 1.5 times the D50 of the lithium metal composite oxide;
(4): a particle size of the adhered fine particles is 0.01 to 0.1 times the D50 of the lithium metal composite oxide; and
(5): an average number of the adhered fine particles adhered per particle of the single particles is 1 or more and 30 or less as measured with respect to a range observable in an image obtained by scanning electron microscope.