US 12,729,434 B2
Method for filling a gap in a three-dimensional structure on a semiconductor substrate
KiKang Kim, Yongin-si (KR); Hak-Yong Kwon, Yongin-si (KR); HieChul Kim, Hwaseong-si (KR); SungKyu Kang, Hwaseong-si (KR); SeungHwan Lee, Anseong-si (KR); SungBae Kim, Yongin-si (KR); JongHyun Ahn, Hwaseong-si (KR); SeongRyeong Kim, Hwaseong-si (KR); KyuMin Kim, Anyang-si (KR); and YoungMin Kim, Hwaseong-si (KR)
Assigned to ASM IP Holding B.V., Almere (NL)
Filed by ASM IP Holding B.V., Almere (NL)
Filed on Oct. 10, 2023, as Appl. No. 18/378,403.
Application 18/378,403 is a continuation of application No. 17/236,782, filed on Apr. 21, 2021, granted, now 11,814,728.
Claims priority of provisional application 63/014,916, filed on Apr. 24, 2020.
Prior Publication US 2024/0043997 A1, Feb. 8, 2024
This patent is subject to a terminal disclaimer.
Int. Cl. C23C 16/455 (2006.01); C23C 16/56 (2006.01); H10P 14/60 (2026.01); H10P 50/24 (2026.01)
CPC C23C 16/45536 (2013.01) [C23C 16/56 (2013.01); H10P 14/6339 (2026.01); H10P 50/242 (2026.01)] 20 Claims
OG exemplary drawing
 
1. A method of filling a gap in a three-dimensional structure on a substrate, the method comprising:
depositing a thin film for filling the gap in the three-dimensional structure using a reaction gas activated with a first radio frequency (RF) power having a first frequency to form a deposited thin film;
performing an etching process, the etching process comprising an etching step and a purge step after the etching step, wherein the etching step comprises providing an etchant comprising fluorine and activating the etchant with a second RF power having a second frequency lower than the first frequency, wherein the deposited thin film is etched during the etching step, wherein the etchant is continuously provided during the etching step, wherein the second frequency is in a range of about 3 kHz to about 1,000 kHz; and
repeating a cycle of the depositing and the etching at least once to form a thin film pattern that fills the gap to a level above a top surface the structure,
wherein the deposited thin film formed on the top surface of the structure and a top portion of the gap are etched more than the deposited thin film formed on a middle surface of the gap and a lower surface of the gap, and
wherein a ratio of voids to material in a volume of the thin film is 0.005 or less.