US 12,729,333 B2
Powder material for sintering and solid latent heat storage member including the same
Asaya Fujita, Nagoya (JP); Hiroyuki Nakayama, Nagoya (JP); Yoshiaki Kinemuchi, Nagoya (JP); Kimihiro Ozaki, Nagoya (JP); and Haruka Abe, Tsukuba (JP)
Assigned to NATIONAL INSTITUTE OF ADVANCED INDUSTRIAL SCIENCE AND TECHNOLOGY, Tokyo (JP)
Appl. No. 17/420,737
Filed by NATIONAL INSTITUTE OF ADVANCED INDUSTRIAL SCIENCE AND TECHNOLOGY, Tokyo (JP)
PCT Filed Dec. 4, 2019, PCT No. PCT/JP2019/047453
§ 371(c)(1), (2) Date Jul. 6, 2021,
PCT Pub. No. WO2020/144982, PCT Pub. Date Jul. 16, 2020.
Claims priority of application No. 2019-001522 (JP), filed on Jan. 9, 2019.
Prior Publication US 2022/0064510 A1, Mar. 3, 2022
Int. Cl. C09K 5/06 (2006.01); C01G 31/02 (2006.01); F28D 20/02 (2006.01)
CPC C09K 5/063 (2013.01) [C01G 31/02 (2013.01); F28D 20/02 (2013.01); C01P 2002/52 (2013.01); C01P 2002/72 (2013.01); C01P 2004/03 (2013.01); C01P 2006/32 (2013.01)] 5 Claims
OG exemplary drawing
 
1. A solid latent heat storage member comprising a bulk body obtained by pressurized sintering a powder material in a vacuum atmosphere so that powder particles of the powder material are directly bonded each other to form the bulk body,
the powder material comprising vanadium and oxygen as main components, wherein the powder material comprises a VO2-based vanadium oxide and one or more types of vanadium oxides other than the VO2-based vanadium oxide, the VO2-based vanadium oxide containing an oxide obtained by partial substitution of V of an oxide represented by a chemical formula VO2 with one or more substitution elements of W, Cr and Al, and having a proportion of the partial substitution of more than 0 atomic % and 20 atomic % or less, wherein, when ratio of sum of atomic % of the vanadium and the substitution elements to atomic % of the oxygen in all powder is expressed as 1:(2+d), d is 0<d<0.1,
a surface of the powder has been oxidized by heating in an air atmosphere so that the surface of the powder comprises a V2O5-based vanadium oxide,
a latent heat quantity per volume of the solid latent heat storage member is 100 J/cc or more,
the bulk body has a foam-like pattern structure, which is observed by a scanning electron microscope, inside,
a relative density of the bulk body based on the density of VO2 is 90% or more, and
a compression strength of the bulk body is 46 MPa or higher.