US 12,729,321 B2
Floor protection system with high dynamic crack bridging
Jochen Grötzinger, Schwäbisch Gmünd (DE); Uwe Von Der Brüggen, Meckesheim (DE); Oguz Sarioglu, Heilbronn (DE); and Edis Kasemi, Zürich (CH)
Assigned to SIKA TECHNOLOGY AG, Baar (CH)
Appl. No. 18/024,908
Filed by SIKA TECHNOLOGY AG, Baar (CH)
PCT Filed Nov. 8, 2021, PCT No. PCT/EP2021/080924
§ 371(c)(1), (2) Date Mar. 6, 2023,
PCT Pub. No. WO2022/096707, PCT Pub. Date May 12, 2022.
Claims priority of application No. 20206557 (EP), filed on Nov. 9, 2020.
Prior Publication US 2023/0312975 A1, Oct. 5, 2023
Int. Cl. C09D 175/00 (2006.01); C09D 7/63 (2018.01); C09D 163/00 (2006.01)
CPC C09D 175/00 (2013.01) [C09D 7/63 (2018.01); C09D 163/00 (2013.01)] 14 Claims
 
1. A floor protection system configured to be applied to a floor substrate and comprising in order from a floor substrate side:
(i) optionally at least one epoxy resin primer,
(ii) at least one polyurethane coating,
(iii) optionally quartz sand, scattered into and/or onto the polyurethane coating, and
(iv) an epoxy resin seal obtained from a resin component containing at least one liquid epoxy resin and a curing agent component containing at least one amine of the formula (I)
Z—NH-A-NH—CH2—Y  (I)
where
A is a divalent C2 to C15 alkylene, cycloalkylene or arylalkylene radical optionally containing one or more nitrogen atoms or ether groups,
Z is H or —CH2—Y and
Y is H or a C1 to C11 alkyl, cycloalkyl, arylalkyl or aryl radical,
wherein the two nitrogen atoms to which the A radical is bonded are separated from one another by at least two carbon atoms, and the amine of the formula (I) contains a total of at least 8 carbon atoms, and
wherein the polyurethane coating consists of one or more layers, and at least one of these layers has an elongation at break of at least 300%, determined at 23° C. to DIN EN 53504 at a strain rate of 200 mm/min.