US 12,729,307 B2
Thermal debonding of primer-initiated curable structural adhesive films
Alexander J. Kugel, Woodbury, MN (US); Dean A. Miner, Prescott, WI (US); Matthew T. Holbrook, Little Canada, MN (US); Nicholas W. Lang, Minnetonka, MN (US); Kristen L. Bellmer, Cottage Grove, MN (US); and Scott M. Spear, St. Paul, MN (US)
Assigned to 3M INNOVATIVE PROPERTIES COMPANY, St. Paul, MN (US)
Appl. No. 17/802,839
Filed by 3M INNOVATIVE PROPERTIES COMPANY, St. Paul, MN (US)
PCT Filed Mar. 3, 2021, PCT No. PCT/IB2021/051782
§ 371(c)(1), (2) Date Aug. 26, 2022,
PCT Pub. No. WO2021/176376, PCT Pub. Date Sep. 10, 2021.
Claims priority of provisional application 62/986,316, filed on Mar. 6, 2020.
Prior Publication US 2023/0088278 A1, Mar. 23, 2023
Int. Cl. C09D 5/00 (2006.01); B32B 43/00 (2006.01); C09D 133/08 (2006.01); C09J 5/06 (2006.01)
CPC C09D 5/002 (2013.01) [B32B 43/006 (2013.01); C09D 133/08 (2013.01); C09J 5/06 (2013.01); B32B 2309/02 (2013.01)] 20 Claims
 
1. A method comprising:
a) providing a bound article comprising, in order:
i) a first adherend;
ii) a first primer layer;
iii) an adhesive layer;
iv) optionally a second primer layer; and
v) a second adherend;
b) heating the article to a release temperature; and
c) separating the first and second adherends such that they are no longer bound together by the adhesive layer;
wherein the release temperature is a temperature between 100° C. and 150° C.;
wherein the adhesive layer exhibits an overlap shear of greater than 1.0 MPa (145 psi) at room temperature, as measured by the Overlap Shear test method described herein; and