| CPC C08L 51/08 (2013.01) [A61C 7/08 (2013.01); A61K 6/893 (2020.01); A61K 6/90 (2020.01); B29C 64/135 (2017.08); B33Y 10/00 (2014.12); B33Y 30/00 (2014.12); B33Y 70/00 (2014.12); B33Y 80/00 (2014.12); C08L 75/16 (2013.01); A61C 2201/00 (2013.01); B29K 2033/08 (2013.01); B29L 2031/753 (2013.01)] | 20 Claims |

|
1. An orthodontic article comprising the reaction product of a polymerizable composition, the polymerizable composition comprising:
a) at least 35 wt. % and no greater than 70 wt. % of one or more monofunctional (meth)acrylate monomers comprising a cyclic moiety, based on the total weight of organic components of the polymerizable composition, wherein at least one of the one or more monofunctional (meth)acrylate monomers is characterized by a homopolymer Tg of at least 60° C., and wherein the polymerizable composition comprises one or more monofunctional (meth)acrylate monomers having a log P value of less than 3 in a total amount of no greater than 10 wt. % of the total monofunctional (meth)acrylate monomers; and
b) a urethane (meth)acrylate polymer comprising polymerized units of an aliphatic polyester diol,
wherein the orthodontic article is an orthodontic alignment tray,
wherein a total amount of monofunctional (meth)acrylate monomers is no greater than 70 wt. %, based on the total weight of organic components of the polymerizable composition,
wherein the reaction product is characterized by a peak tan delta temperature of greater than 60° C., as determined according to dynamic mechanical analysis at a temperature sweep at a rate of 2° C./min from −60° C. to 200° C. after conditioning in deionized water at 37° C. for 24 hours, and
wherein the Tg is measured by Differential Scanning calorimetry at a heating rate of 10° C. per minute.
|